KH-207 is a new type of liquid retarding water reducer. Through the optimization of the synthetic formulation, the prepared concrete exhibits excellent slump retention.
KH-207 complies with The ASTM C 494 Norm
ASTM C 494, Type D
Advantages:
·High Plasticity Retention: It has excellent slump retention, significantly extends the construction operable time, and reduces the time loss of concrete fluidity.
·High Compatibility: It has excellent dispersion capabilities for different types of cement, and can delay or inhibit the hydration of cement.
·High Durability: It enhances the compactness of the hardened slurry, improves shrinkage and creep performance, reduces cracks, and improves durability.
·Eco Friendly: Does not contain harmful substances, safe and environmentally friendly.
Technical Data:
| KH-207 Main Specifications | ||||
| NO | Test Item | Criterion | Detection result | |
| 1 | Appearance and color | Colorless transparent or light yellow liquid | Colorless transparent or light yellow liquid | |
| 2 | Water reduction rate /% | ≥25 | 29 | |
| 3 | Solid content (%) | 30~50±1.0 | 40~50±1.0 | |
| 4 | Slurry fluidity (mm) | ≥220 | 240 | |
| 5 | Compressive strength ratio (%) | 1d | / | / |
| 3d | / | / | ||
| 7d | ≥140 | 147 | ||
| 28d | ≥130 | 140 | ||
| 6 | Gas content /% | ≤6.0 | 2.2 | |
| 7 | pH value (20℃) | 6~8 | 7.0 | |
| 8 | Density/(g/cm3) | 1.06~1.15 | 1.10 | |
| 9 | Reinforcement corrosion | The presence of corrosion hazards should be indicated | No | |
| 10 | validity | / | 6 months | |
| 11 | package | / | IBC ton barrel, 1000kg/ barrel | |
| 12 | store | / | Store in a dry and ventilated place, away from direct sunlight | |
Product application:
KH-207 is suitable for various silicate series cement concrete systems. Such as in:
Concrete that needs to maintain its working performance for a long time.
Uses:
1.KH207 can be measured and added to the concrete along with the mixing water directly; it can also be diluted to a lower solid content, and then added to the concrete in corresponding amounts.
2.The recommended dosage is 0.4-1.0% of the cementitious material. The exact dosage should be determined after trial mixing, based on concrete design requirements and actual raw material conditions.
3.It should be used with KH-204 polycarboxylic acid superplasticizer;